SUPER DUPLEX 2507 High Quality

Product Detail

Product Tags

A 22Cr-3Mo Stainless Steel

● Sheet
● Plate
● Bar
● Pipe & Tube (welded & seamless)
● Fittings
● Elbows, tees, stub-ends, returns, caps, crosses, reducers, pipe nipples, etc.
● Weld Wire AWS ER2594, E2594-16, E2553T-1

Duplex 2507 Overview

Inconel 718 welded pipe

Duplex 2507 is a super duplex stainless steel designed for applications which demand exceptional strength and corrosion resistance. Alloy 2507 has 25% chromium, 4% molybdenum, and 7% nickel. This high molybdenum, chromium and nitrogen content results in excellent resistance to chloride pitting and crevice corrosion attack and the duplex structure provides 2507 with exceptional resistance to chloride stress corrosion cracking.

Usage of Duplex 2507 should be limited to applications below 600° F (316° C). Extended elevated temperature exposure can reduce both the toughness and corrosion resistance of alloy 2507.

Duplex 2507 possesses excellent mechanical properties. Often a light gauge of 2507 material can be used to achieve the same design strength of a thicker nickel alloy. The resulting savings in weight can dramatically reduce the overall cost of fabrication.

Corrosion Resistance

2507 Duplex is highly resistant to uniform corrosion by organic acids such as formic and acetic acid. It is alsohighly resistant to inorganic acids, especially if they contain chlorides.  Alloy 2507 is highly resistant to carbide-related intergranular corrosion.  Due to the ferritic portion of the duplex structure of the alloy it is very resistant to stress corrosion cracking in warm chloride containing environments. Through additions of chromium, molybdenum and nitrogen localized corrosion such as pitting and crevice attack are improved. Alloy 2507 has excellent localized pitting resistance.

Hastelloy C2000 bars

What are the characteristics of Duplex 2507?

● High resistance to chloride stress corrosion cracking
● High Strength
● Superior resistance to chloride pitting and crevice corrosion
● Good general corrosion resistance
● Suggested for applications up to 600° F
● Low rate of thermal expansion
● Combination of properties given by austenitic and ferritic structure
● Good weldability and workability

Chemical Composition, %

Cr

Ni

Mo

C

N

Mn

Si

Cu

P

S

Fe

24.0-26.0

6.0-8.0

3.0-5.0

0.030 Max

.24-.32

1.20 Max

0.80 Max

0.50 Max

0.035 Max

0.020 Max

Balance

In what applications is Duplex 2507 used?

● Desalination Equipment
● Chemical process pressure vessels, piping and heat exchangers
● Marine Applications
● Flue Gas Scrubbing Equipment
● Pulp & Paper Mill Equipment
● Offshore Oil production/technology
● Oil and gas industry equipment

ASTM Specifications

Pipe Smls

Pipe Welded

Tube Smls

Tube Welded

Sheet/Plate

Bar

Flanges & Fittings

A790

A790

A789

A789

A240

A276

A182

Mechanical Properties

Specified Tensile Properties, Plate ASTM A240

Ultimate Tensile Strength, ksi

Minimum .2% Yield Strength, ksi Minimum

% Elongation Min.

Hardness (HRB) Max.

116

80

15

310

Alloy 2205 Duplex Stainless Plate (5)
Alloy 2205 Duplex Stainless Plate (1)
asd
asd

  • Previous:
  • Next:

  • Write your message here and send it to us