Nickel

  • Nickel

    High Temperature Alloy Chemical composition Grade Ni Fe Cu C Mn S Si Nickel200 99 ≤0.4 ≤0.25 ≤0.15 ≤0.35 ≤0.01 ≤0.35 Nickel201 99 ≤0.4 ≤0.25 ≤0.02 ≤0.35 ≤0.01 ≤0.35 Alloy property minimum product form condition tensile strength RmN/m㎡ Yield Strength Rp0.2N/m㎡ Elongation As% Brinell hardness HB stick and strip hot rolled 60~85 15~45 35~55 45~80 stick and strip cold drawn or annealed 55~75 15...