Nimonic

Product Detail

Product Tags

High Temperature Alloy

◆ Nimonic90 has high tensile strength and creep resistance, good oxidation resistance and corrosion resistance, and is suitable for turbine discs, blades and high-temperature fasteners of turbine engines.
◆ Nimonic91 has high strength and anti-oxidation performance at high temperature of 650-1000°C, and is suitable for high-temperature components such as aero-engine blades, rocket engines, and nuclear power.

Chemical composition

Grade

C

Si

Mn

S

P

Cr

Ni

Fe

Cu

Ti

Al

Co

other

no greater than

Nimonic90

0.13

1

1

0.015

 

18~21

base

≤1.5

≤0.2

2~3

1~2

15~21

lead≤0.002      B≤0.02        Zr≤0.15

Nimonic91

0.1

1

1

0.015

 

27~30

base

≤1

≤0.5

1.9~2.7

0.9~1.5

19~21

Nb0.4~1.1  B0.002~0.01  Zr≤0.1

Alloy property minimum

Grade

state

tensile strength RmN/m㎡

Yield Strength Rp0.2N/m㎡

Elongation As%

Brinell hardness HB

Nimonic90

Solution treatment

780

550

7

-

Nimonic91

Solution treatment

820

590

8

-