Monel 400 Uns N04400 W.Nr. 2.4360 And 2.4361
Chemical Composition
Alloy |
element |
C |
Si |
Mn |
S |
Ni |
Fe |
Cu |
Monel 400 |
Min |
63.0 |
28.0 |
|||||
Max |
0.3 |
0.5 |
2.0 |
0.024 |
2.5 |
34.0 |
Mechanical Properties
Aolly Status |
Tensile strength Rm Mpa Min |
Yield strength R P 0. 2 Mpa Min |
Elongation A 5 % Min |
Solution |
745 |
325 |
40 |
Physical Properties
Aolly Status |
Tensile strength Rm Mpa Min. |
Yield strength R P 0. 2 Mpa Min. |
Elongation A 5 % |
annealed |
480 |
170 |
35 |
Standard
Rod, Bar, Wire and Forging Stock - ASTM B 164 (Rod, Bar, and Wire),ASTM B 564 (Forgings)
Plate, Sheet and Strip -,ASTM B 127, ASME SB 127
Pipe & Tube - ASTM B 165(Seamless Pipe and Tube), ASTM B 725 (Welded Pipe), ASTM B 730 (Welded Tube), ASTM B 751 (Welded Tube), ASTM B 775 (Welded Pipe), ASTM B 829(Seamless Pipe and Tube)
Welding Products - Filler Metal 60-AWS A5.14/ERNiCu-7;Welding Electrode 190-AWS A5.11/ENiCu-7.
![Incoloy926 is an austenitic stainless steel with similar chemical composition to alloy 904L, its nitrogen content is increased to about 0.2%, and its molybdenum content is 6.5%.](http://www.hnsuperalloys.com/uploads/N08367-1.4529-Incoloy-926-bars2.jpg)
Characteristics of Monel 400
![Inconel 600 bars](http://www.hnsuperalloys.com/uploads/Inconel-600-bars1.jpg)
● Resistant to seawater and steam at high temperatures
● Excellent resistance to rapidly flowing brackish water or seawater
● Excellent resistance to stress corrosion cracking in most freshwaters
● Particularly resistant to hydrochloric and hydrofluoric acids when they are de-aerated
● Offers some resistance to hydrochloric and sulfuric acids at modest temperatures and concentrations, but is seldom the material of choice for these acids
● Excellent resistance to neutral and alkaline salt
● Resistance to chloride induced stress corrosion cracking
● Good mechanical properties from sub-zero temperatures up to 1020° F
● High resistance to alkalis
● Previous: Alloy N-155
● Next: Monel k-500 UNS N05500/ W.Nr. 2.4375
![Alloy 2205 Duplex Stainless Plate (3)](http://www.hnsuperalloys.com/uploads/Alloy-2205-Duplex-Stainless-Plate-3.jpg)
![Alloy 2205 Duplex Stainless Plate (5)](http://www.hnsuperalloys.com/uploads/Alloy-2205-Duplex-Stainless-Plate-5.jpg)
![vcavs (4)](http://www.hnsuperalloys.com/uploads/vcavs-42.png)
![vcavs (1)](http://www.hnsuperalloys.com/uploads/vcavs-12.png)